Effect Of Plastic Flow And Volume Changes On Design

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect Of Plastic Flow And Volume Changes On Design

Author(s): Clyde T. Morris

Publication: Journal Proceedings

Volume: 33

Issue: 11

Appears on pages(s): 123-128

Keywords: none

DOI: 10.14359/8411

Date: 11/1/1936

Abstract:
It is recognized that concrete changes in volume when subjected to stress (elastic deformation), sustained load (plastic flow), changes in moisture con-tent (shrinkage), and temperature changes. Formulas are given for estimating changes due to plastic flow and their effect on deflections, stress in the steel and stress in the concrete.