Metallic Aggregate In Concrete Floors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Metallic Aggregate In Concrete Floors

Author(s): Edward W. Scripture

Publication: Journal Proceedings

Volume: 33

Issue: 9

Appears on pages(s): 17-27

Keywords: none

DOI: 10.14359/8406

Date: 9/1/1936

Abstract:
The requirements of metallic aggregate for use in concrete floors are given and good practice in laying floors with such aggregates is described. Methods and apparatus for measuring the resistance to abrasion and to impact are described. The results secured show the superiority of leaner mixes contain-ing aggregate of larger maximum size of metallic aggregate at the surface and of encreasing the thickness of the metallic layer. Comparisons of mechanical floating and tamping are made.