A Study Of The Economics Of High Strength Concrete In Building Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Study Of The Economics Of High Strength Concrete In Building Construction

Author(s): F. E. Richart

Publication: Journal Proceedings

Volume: 32

Issue: 3

Appears on pages(s): 459-472

Keywords: none

DOI: 10.14359/8392

Date: 3/1/1936

Abstract:
An analysis, using average current prices of concrete and steel, of savings to be effected by the use of high strength concrete in building construction. Studies of beams, footings areslabs, flat slabs, columns, and included. Considerable savings are theoretically possible in columns, smaller savings in flexural members, except as dead load can be reduced. While the greatest savings could be effected by using high strength concrete and higher steel stresses, the undesirability of the latter is discussed.