Slabs Supported On Four Sides

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Slabs Supported On Four Sides

Author(s): J. Di Stasio and M. P. Van Buren

Publication: Journal Proceedings

Volume: 32

Issue: 1

Appears on pages(s): 350-364

Keywords: none

DOI: 10.14359/8387

Date: 1/1/1936

Abstract:
The basis of the ACI Building Regulations for slabs supported on four sides is covered in this paper. Factors of equivalent uniformly distributed loads are determined for use in calculating bending moments and shears in each direction of the slabs and supporting beams. With these factors, the design of slabs with any degree of rectangularity or variation in adjacent panels may be handled in the same manner as in one-way construction. A minimum thickness formula is establlshed based on limiting deflection to definite ratios of the span consistent with all cases of rectangularity and continuity.