Title: Concrete By Pump And Pipeline

Author(s): Charles F. Ball

Publication: Journal Proceedings

Volume: 32

Issue: 1

Appears on pages(s): 333-349

Keywords: none

DOI: 10.14359/8386

Date: 1/1/1936

Abstract:
A description and explanation of the Pumpcrete (concrete pump) system with an analysis of the specific and unusual problems encountered in pumping plastic concrete mixtures, and the devices employed to meet these problems. A discussion of various mixtures that have been pumped, with some conclusions about concrete components and proportions that affect pumpability, is included.