Uniformity Of Concrete On The Average Job-A Study Of 13,000 Field Tests

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Uniformity Of Concrete On The Average Job-A Study Of 13,000 Field Tests

Author(s): Hugh C. Ross

Publication: Journal Proceedings

Volume: 32

Issue: 1

Appears on pages(s): 277-284

Keywords: none

DOI: 10.14359/8381

Date: 1/1/1936

Abstract:
An analysis is presented of 13,000 concrete compression tests from 60 different job operations. The data show what variations in strength are likely to be encountered on the average job and the extent to which these variations are affected by the class of concrete involved. Curves illustrate how overdesigning will reduce the number of substandard tests and what margin of strength should be provided to meet given quality requirements.