Load Performance Tests Of Precast Joist-Precast Slab Floor Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Load Performance Tests Of Precast Joist-Precast Slab Floor Construction

Author(s): R. E. Copeland

Publication: Journal Proceedings

Volume: 32

Issue: 11

Appears on pages(s): 195-211

Keywords: none

DOI: 10.14359/8377

Date: 11/1/1935

Abstract:
The tests reported herein were conducted on a type of Iightweight concrete floor constructed of precast reinforced concrete slab sections laid on and united to precast reinforced concrete joists. The type of bond joint between the slab and joist was an important factor of panel strength and performance. The performance of the panels also indicated that it was possible and practicable to construct precast joist-precast slab floors in such a manner that the joist and slab function together as a T-section.