The Mechanics Of Plastic Flow Of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Mechanics Of Plastic Flow Of Concrete

Author(s): J. R. Shank

Publication: Journal Proceedings

Volume: 32

Issue: 11

Appears on pages(s): 149-180

Keywords: none

DOI: 10.14359/8374

Date: 11/1/1935

Abstract:
A parabolic type of equation is found to closely express the time-deformation curve for plastic flow. Test data available are summarized and tabulated giving the coefficients and exponents for the curves. These data are studied and quantitative values are given affect plastic flow. to express the conditions that on this are developed exact expressions for reinforced concrete column stresses after a certain period for sustained load and also for sustained strain. Approximate procedures are given for beams. Some space is given to similar expressions for shrinkage.