Mosaic Ceilings, U. S. Department Of Justice Building

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mosaic Ceilings, U. S. Department Of Justice Building

Author(s): John J. Earley

Publication: Journal Proceedings

Volume: 31

Issue: 5

Appears on pages(s): 557-564

Keywords: none

DOI: 10.14359/8364

Date: 5/1/1935

Abstract:
A description of the design and construction of mosaic ceilings. The impervious precast concrete slabs were used as forms into which the structural concrete was placed, saving the cost of wood formsand being more rigid than any wooden framework.