Construction Features Of The Zeiss Dywidag Dome For The Hayden Planetarium Building

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction Features Of The Zeiss Dywidag Dome For The Hayden Planetarium Building

Author(s): R. L. Bertin

Publication: Journal Proceedings

Volume: 31

Issue: 5

Appears on pages(s): 449-460

Keywords: none

DOI: 10.14359/8355

Date: 5/1/1935

Abstract:
A brief history of the evolution of curved struc- tures is given as an introduction to the description of the construction of the dome for the Hayden Plane- tarium. The Zeiss-Dywidag dome for the planetarium is a hemisphere, 8 ft 6 in, in diameter on the in- side, the shell is 3 in. thick. In constructing the form- work, a self-supporting structure was adopted which would follow the geometrical characteristics of a sphere.