Compressive Strength Prediction of Hollow Concrete Block Masonry Prisms

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compressive Strength Prediction of Hollow Concrete Block Masonry Prisms

Author(s): K. Ramamurthy, V. Sathish, and R. Ambalavanan

Publication: Structural Journal

Volume: 97

Issue: 1

Appears on pages(s): 61-67

Keywords: compressive strength; concrete blocks; masonry; mortars (material); prisms; tests.

DOI: 10.14359/834

Date: 1/1/2000

Abstract:
This paper discusses the results of a systematic experimental investigation on 306 stretcher bonded concrete hollow block masonry prisms under axial compression for the influences of block-mortar strength combinations, block geometry, height to thickness ratio (h/t) of block, mortar bedding, and thickness of mortar joint. The test results are then used to derive a prediction relation for a rational assessment of the compressive strength of masonry prisms.