Lightweight Slag Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Lightweight Slag Concrete

Author(s): Inge Lyse

Publication: Journal Proceedings

Volume: 31

Issue: 9

Appears on pages(s): 1-7

Keywords: none

DOI: 10.14359/8334

Date: 9/1/1934

Abstract:
Tests of concrete containing porous slag as coarse aggregate and natural sand as fine are described. The weight of the concrete was reduced considerably by the porous slag. Compressive, flexural and diagonal tension strengths as well as bond strengths and -modulus of elasticity of the concrete were nearly the same for slag as for gravel aggregates.