Tendencies In Canadian Railway Bridge Design- Recent Work On The Canadian National Railways

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tendencies In Canadian Railway Bridge Design- Recent Work On The Canadian National Railways

Author(s): H. S. Van Scoyoc

Publication: Journal Proceedings

Volume: 30

Issue: 5

Appears on pages(s): 465-478

Keywords: none

DOI: 10.14359/8329

Date: 5/1/1934

Abstract:
Developments in bridge design made by the Canadian National Railways, Canada from 1921 t o 1934 are described. These Include (I) simple beam cast-in-place, (2) simple beam precast, (3) span continuous over center support, cast-in-place with concrete ties, (4 precast beam continuous over center support, center 15) rigid frame, continuous over support, rigid frame, cast-in-place cast-in- lace (6) single and (7) through without ties or ballast. beams, carrying reinforce, with steel floor: without ties or ballast. concrete T-section slab Special emphasis is placed on reduction in height required from top of roadway to top of rail by omission of ties and ballast.