Title: Architectural Concrete Of The Exposed Aggregate Type

Author(s): John J. Earley

Publication: Journal Proceedings

Volume: 30

Issue: 3

Appears on pages(s): 251-278

Keywords: none

DOI: 10.14359/8314

Date: 3/1/1934

Abstract:
This paper is a continuation of "The Project of Ornamenting the Baha’i Temple Dome," ACI Journal, June 1933. Describes some of the techniques by which architectural concrete of the exposed age methods has been developed and some of the which the ornamentation of the Temple has been done.