Proper Methods Of Design And Construction Of Concrete Structures To Prevent Damage From Volumetric Changes Of the Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proper Methods Of Design And Construction Of Concrete Structures To Prevent Damage From Volumetric Changes Of the Concrete

Author(s): G. E. Troxell

Publication: Journal Proceedings

Volume: 30

Issue: 1

Appears on pages(s): 209-230

Keywords: none

DOI: 10.14359/8310

Date: 1/1/1934

Abstract:
Summarizes known information concerning volume changes of concrete, outlines research required to determine the unknown effect of certain factors on volume changes, and indicates how damage of structures due to volume changes may be at least partially prevented by proper choice of materials used and proportioning of the mix, by correct design of the structure, and by proper construction methods.