Selecting Concrete Plant-Meadowbrook Hospital

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Selecting Concrete Plant-Meadowbrook Hospital

Author(s): John G. Ahlers

Publication: Journal Proceedings

Volume: 30

Issue: 11

Appears on pages(s): 142-152

Keywords: none

DOI: 10.14359/8306

Date: 11/1/1933

Abstract:
An analysis of four types of concrete plant for a scattered group of hospital buildings presents an approach to the problem of selection of the best and most economical type . Final, reasoning leading to a central plant and distribution of concrete by special truck, hopper type, concludes the paper.