The Project Of Ornamenting The Baha'I Temple Dome

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Project Of Ornamenting The Baha'I Temple Dome

Author(s): John J. Earley

Publication: Journal Proceedings

Volume: 29

Issue:

Appears on pages(s): 403-411

Keywords: none

DOI: 10.14359/8285

Date: 6/1/1933

Abstract:
A discussion of the problems faced in ornamenting the Baha’i Temple dome. A full-size model of the dome was constructed in the studio prior to casting the architectural concrete slabs.