Vibratory Finishing Machine For Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Vibratory Finishing Machine For Concrete Pavements

Author(s): F. V. Reagel

Publication: Journal Proceedings

Volume: 29

Issue:

Appears on pages(s): 391-396

Keywords: none

DOI: 10.14359/8283

Date: 6/1/1933

Abstract:
A vibrating-screed type finishing machine and a standard type Ord, finisher were used in a series of tests on a concrete paving project. The results of the tests definitely indicate that leaner mixes can be satisfactorily finished by the vibratory method without sacrificing quality of the concrete. This indicates that a potential saving in the cost of materials can be effected.