Title: An 8-Hour Accelerated Strength Test For Field Concrete Control

Author(s): O. G. Patch

Publication: Journal Proceedings

Volume: 29

Issue:

Appears on pages(s): 318-324

Keywords: none

DOI: 10.14359/8276

Date: 3/1/1933

Abstract:
Describes a practical method of determining the potential 28-day strength of concrete within 8 hr after mixing. The method is valuable in predicting the effect of changes in mixes, as well as in calling attention to gradual changes in strength due often to otherwise unrecognized conditions and is also helpful in mix design.