Title: Sliding Form Work

Author(s): W. R. Sproul

Publication: Journal Proceedings

Volume: 29

Issue:

Appears on pages(s): 285-299

Keywords: none

DOI: 10.14359/8274

Date: 2/1/1933

Abstract:
Data and descriptions are presented of methods in applications of sliding forms, especially in reference to rectangular structures of high, clear story height and free standing single and double walls, as employees cold storage for ice storage. The basic principles of operation and erection are similar to those employed in erection of grain elevators. Drawings are Included,