Title: Concreting Problems-Chats Falls Power Development

Author(s): H. L. Trotter and Wilfrid Schnarr

Publication: Journal Proceedings

Volume: 29

Issue:

Appears on pages(s): 249-274

Keywords: none

DOI: 10.14359/8272

Date: 2/1/1933

Abstract:
Describes a powerhouse and 3 miles of a dam, the aggregates, proportions, plant, and transportation. The duties of the inspectors and the field laboratory are outlined. Details in placing monolithic concrete, and summer and winter curing are outlined, while experimental data as to the temperature and artificial cooling of concrete are discussed.