Sliding Form Work

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Sliding Form Work

Author(s): L. Boyd Mercer

Publication: Journal Proceedings

Volume: 29

Issue:

Appears on pages(s): 201-240

Keywords: none

DOI: 10.14359/8271

Date: 1/1/1933

Abstract:
to A practical description of the procedure and pitfalls be met in the construction and operation of sliding forms. Various types of ja cks and the methods for con- necting through them to the formwork and operating platform are described in detail. Organization of labor and plant are discussed and while outlining the econo- mies of this method of construction the report stresses the need for considering sliding forms as a flexible machine ca supervisor. T able of presenting many worries for the factors he report concludes with a survey of prac- which must receive consideration when design ing concrete work for construction with sliding