Central Concrete Mixing Plant, Puget Sound Navy Yard

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Central Concrete Mixing Plant, Puget Sound Navy Yard

Author(s): A. O. Hunter

Publication: Journal Proceedings

Volume: 29

Issue:

Appears on pages(s): 81-85

Keywords: none

DOI: 10.14359/8265

Date: 10/1/1932

Abstract:
Describes the plant used to supply ready-mixed con- crete and crushed stone for the navy yard The plant layout is described and the economies obtained com-T with th a previous costs under other conditions use of bulk cement is important and this feature contributes largely to the economy and reliability of the plant.