The Physical Properties Of Cast Stone

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Physical Properties Of Cast Stone

Author(s): John Tucker, JR., G. W. Walker and J. Arthur

Publication: Journal Proceedings

Volume: 28

Issue: 12

Appears on pages(s): 243-264

Keywords: none

DOI: 10.14359/8239

Date: 12/1/1931

Abstract:
A report of results of tests made as basis from which the Federal S ecification for Cast Stone was prepared. The 68 samp es were representative of all the usual methods of fabrication and included a wide variety of aggregate. The strengths, absorption properties, and resistance to freezing and thawing were determined. The compressive strengths varied from I558 to 21,720 the 48-hr absorption from 2.0 to 13.1 percent. Resistance to freezing and thawing varied from complete disintegration at 25 cycles to the first signs of disintegration at 1450 cycles.