Field Practices In Using Concrete Aggregates In Multiple Sizes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Field Practices In Using Concrete Aggregates In Multiple Sizes

Author(s): T. C. Thee

Publication: Journal Proceedings

Volume: 27

Issue: 6

Appears on pages(s): 1203-1227

Keywords: none

DOI: 10.14359/8223

Date: 6/1/1931

Abstract:
Field practices using multiple sizes of aggregate in having operations are cited. This separation of sizes elps eliminate segregation in transportation and stock piling. Cost and time study data are given for two-and three-way batching used in paving operations as well as plant layouts for the handling of multiple size aggregates.