Title: Studies of Concrete Mixtures

Author(s): S. C. Hollister

Publication: Journal Proceedings

Volume: 27

Issue: 4

Appears on pages(s): 959-974

Keywords: none

DOI: 10.14359/8211

Date: 4/1/1931

Abstract:
In the course of concrete mixing and placing, it has been the experience of many that there are occurrences in the behavior of the mixture that are not readily ex-plained by the customary concepts of mixtures. Paper relates and attempts to explain many of the phenomena through the medium of a more detailed concept of the concrete mixture prior to hardening.