Second Progress Report On Column Tests Made At Lehigh University

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Second Progress Report On Column Tests Made At Lehigh University

Author(s): W. A. Slater and Inge Lyse

Publication: Journal Proceedings

Volume: 27

Issue: 3

Appears on pages(s): 791-835

Keywords: none

DOI: 10.14359/8206

Date: 3/1/1931

Abstract:
The first Progress Rport of Committee 105 on Column Investigations was published in the April Journal 1950. That report gives the program of the investigation and results of the preliminary tests of the materials. The first progress report from Lehigh University on the column tests gives results for Series 1 and 2 and was published in the February Journal The present progress report from Lehigh University gives results for Series 3 on columns subjected to working loads for 20 weeks. Wherever references are made to the results for Series 1 and 2 the information will be found in the first progress report.