Cinders As Concrete Aggregate

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cinders As Concrete Aggregate

Author(s): Einar Christensen

Publication: Journal Proceedings

Volume: 27

Issue: 2

Appears on pages(s): 583-646

Keywords: none

DOI: 10.14359/8199

Date: 2/1/1931

Abstract:
A summary of the field of cinder aggregates, from THE nature and properties of cinders to the character- IstIcs of the resulting concrete. The topics covered include: properties of cinder aggregates, specification for cinders, cinder concrete building units, sand-cinder concrete, and properties of cinder and sand-cinder concrete.