Memorandum On Arch Dam Developments

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Memorandum On Arch Dam Developments

Author(s): Lars Jorgensen

Publication: Journal Proceedings

Volume: 27

Issue: 9

Appears on pages(s): 1-64

Keywords: none

DOI: 10.14359/8180

Date: 9/1/1930

Abstract:
Records developments in arch dam design and con- struction with special reference to constant angle arch dam design. Actual cost data have been grven for various structures - covering all kinds of locations as a guide for estimating the cost of new work. When desiqninq an arch dam, the simole arch formulas (unit water pressure X length of upstream radius -unit stress X thickness) is used to obtain a preliminary section. The bending moments and resultin stresses are calculated by Cain’s formulas. Design tab es, l equa- tions, procedures, computations and drawings from various dams are included.