Title: Some Permeability Studies of Concrete

Author(s): F. R. McMillan and Inge Lyse

Publication: Journal Proceedings

Volume: 26

Issue:

Appears on pages(s): 101-142

Keywords: none

DOI: 10.14359/8148

Date: 12/1/1929

Abstract:
A study of some of the factors affecting permeability of concrete as determined by the measurement ofthe water actually passing through as distinct from that entering a given specimen in a given time. Many variables studied included different cements, water-cement ratios, curing periods, ages, and effect of admixtures. The tests show that the method of placing, the moist curing period and water-cement ratio areprincipal factors affecting waterting hotness. The apparatus used is Illustrated.