Title: Construction Specification For Concrete Work On Ordinary Buildings BUILDINGS

Author(s): Arthur R. Lord

Publication: Journal Proceedings

Volume: 26

Issue:

Appears on pages(s): 1-17

Keywords: none

DOI: 10.14359/8142

Date: 11/1/1929

Abstract:
The first of a series of specifications to be prepared and issued under the auspices of the American Con- crete Institute. The specification applies to concrete work in ordinary commercial or industrial buildings.