Rebound in Dry-Mix Shotcrete: Influence of Type of Mineral Admixture

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rebound in Dry-Mix Shotcrete: Influence of Type of Mineral Admixture

Author(s): V. Bindiganavile and N. Banthia

Publication: Materials Journal

Volume: 97

Issue: 2

Appears on pages(s): 115-119

Keywords: carbon black; fly ash; shotcrete; silica fume.

DOI: 10.14359/813

Date: 3/1/2000

Abstract:
The high rebound in dry-mix shotcrete has severe implications both on its long-term durability and the mechanical performance in service. The use of mineral admixtures is often recommended as a way of reducing rebound, but the exact influence of the admixture dosage rate, shape, and mean size of their particles on the rebound is not clearly understood. In the research reported herein, four mineral admixtures—silica fume, fly ash, high reactivity metakaolin, and carbon black—were investigated in plain and fiber-reinforced dry-mix shotcrete for rebound and other properties. These admixtures represent particle sizes ranging from 0.05 to 10 mm and particle shapes ranging from spherical to plate-like. Results indicate that while fly ash is not as effective, both silica fume and carbon black substantially reduce the rebound. The performance of high reactivity metakaolin lies somewhere in between. Overall, it appears that the mean particle size of the admixture influences the rebound far more than the shape of its particles.


ALSO AVAILABLE IN:

Electronic Materials Journal