Behavior of a Continuous Slab Prestressed in Two Directions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of a Continuous Slab Prestressed in Two Directions

Author(s): A. C. Scordelis, T. Y. Lin, and R. Itaya

Publication: Journal Proceedings

Volume: 56

Issue: 12

Appears on pages(s): 441-460

Keywords: none

DOI: 10.14359/8105

Date: 12/1/1959

Abstract:
Elastic behavior and ultimate strength of a continuous concrete slab prestressed in two directions were investigated. The slab, consisting of four panels, was supported at nine points and simulated a flat slab. Prestressing was accomplished by means of unbonded post-tensioned cables. Experimental values for moments, deflections, and reactions were compared with theoretical values’obtained by the elastic plate theory and by approximate theories used in present design methods.