Title: Concrete Technology and Aggregate Production for St. Lawrence Seaway

Author(s): M. R. Smith and Gordon M. kidd

Publication: Journal Proceedings

Volume: 56

Issue: 11

Appears on pages(s): 361-376

Keywords: none

DOI: 10.14359/8101

Date: 11/1/1959

Abstract:
Curing practices and high lift versus low lift construction were sources of the major differences between Canadian and United States practices on the St. Lawrence Seaway. Contrasting materials and mixing specification require- ments are also reported. Both United States and Canadian aggregate production procedures and equipment are detailed.