Fire Resistance of a Prestressed Concrete Floor Panel CONCRETE FLOOR PANEL-.

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fire Resistance of a Prestressed Concrete Floor Panel CONCRETE FLOOR PANEL-.

Author(s): G. E. Troxell

Publication: Journal Proceedings

Volume: 56

Issue: 8

Appears on pages(s): 97-106

Keywords: none

DOI: 10.14359/8085

Date: 8/1/1959

Abstract:
General fire resistance features of conventional reinforced concrete and prestressed concrete are compared. Results are given of a 4-hr standard ASTM fire test on a 16 x 16-ft prestressed floor panel having an edge beam and an interior beam. Both beams and the 6-in. floor slab were post-tensioned and the cables were not grouted. Temperatures at several thermocouples on the steel cables and in the concrete were observed during the test. With a 1 1/2-in. clear protection for the slab cables and a P-in. clear protection for the beam cables no structural failure occurred during the 4-hr fire test. The temperature rise of the top surface of the 6-in. slab exceeded the allowable after 3 hr 51 min