Response of Concrete Shear Keys to Dynamic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Response of Concrete Shear Keys to Dynamic Loading

Author(s): Robert J. Hansen, Edward G. Nawy, and Jayant M. Shah

Publication: Journal Proceedings

Volume: 57

Issue: 5

Appears on pages(s): 1475-1490

Keywords: none

DOI: 10.14359/8073

Date: 5/1/1961

Abstract:
A series of comparative static and dynamic tests on three types of concrete shear keys has been completed. Results indicate that plain concrete shear keys can withstand stresses as high as 2000 psi , that imposing transverse compression on the keys raises the ratio of shear to compressive strength by about 50 percent in the dynamic loading case though by only about 5 percent in the static loading case, and that keys indicate much higher shear strengths when loaded dynamically than statically.