Prestressed Concrete Beams by Electronic Computer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prestressed Concrete Beams by Electronic Computer

Author(s): Charles Wilson

Publication: Journal Proceedings

Volume: 57

Issue: 5

Appears on pages(s): 1459-1474

Keywords: none

DOI: 10.14359/8072

Date: 5/1/1961

Abstract:
Describes the analysis and design of prestressed concrete bridge members as performed by a small-scale electronic computer. Specifically, the member must be a simply supported longitudinal highwqy bridge beam carrying standard AASHO trucks. To demonstrate results of programing, an illustrative problem is presented showing input data, computational effort, and computer results.