Fixed-End Moments in Columns of Asymmetrical Multispan Integral Frames due to Longitudinal Displacements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fixed-End Moments in Columns of Asymmetrical Multispan Integral Frames due to Longitudinal Displacements

Author(s): Shu-T'ien Li

Publication: Journal Proceedings

Volume: 57

Issue: 4

Appears on pages(s): 1373-1386

Keywords: none

DOI: 10.14359/8068

Date: 4/1/1961

Abstract:
Presents a general method for determining fixed-end moments in columns due to thermal changes, shrinkage, and rib-shortening of the monolithically continuous girder in asymmetrical integral bridge frames having different span lengths, column heights, and moments of inertia either constant or variable, and hence it is applicable to any combination of them in any form.