Work of the European Concrete Committee

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Work of the European Concrete Committee

Author(s): Franco Levi

Publication: Journal Proceedings

Volume: 57

Issue: 3

Appears on pages(s): 1041-1070

Keywords: none

DOI: 10.14359/8057

Date: 3/1/1961

Abstract:
Summarizes recommendations approved by the Comite Europeen du Beton (CEB) since its organization in 1953. Among the recommendations reviewed are those on ultimate strength design, T-beams, buckling, cracking, deformation, shearing stress, safety factors, and notation. A brief account of planned activities of CEB is also presented.