Title: Ultimate Strength of a Folded Plate Structure

Author(s): Gregory P. Chacos and John B. Scalzi

Publication: Journal Proceedings

Volume: 57

Issue: 2

Appears on pages(s): 965-972

Keywords: none

DOI: 10.14359/8055

Date: 2/1/1961

Abstract:
Objectives of this investigation were to determine the behavior of the folded plate structure as a simple beam with an irregular cross section and to verify the ultimate moment capacity by the rectangular stress block method. For this type of structure the ultimate collapse load agreed with the theoretical load within 1.8 percent.