Creep of Prestressed Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Creep of Prestressed Concrete Beams

Author(s): W. S. Cottingham, P. G. Fluck, and G. W. Washa

Publication: Journal Proceedings

Volume: 57

Issue: 2

Appears on pages(s): 929-936

Keywords: none

DOI: 10.14359/8052

Date: 2/1/1961

Abstract:
Presents test results obtained during 7 years of sustained loading of six prestressed concrete beams. Each beam was end-supported over a PO-ft span and uniformly loaded. Two beams were loaded to full design load, two were loaded to 3/4 design load, and two were loaded to 1/2 design load. Creep deflections and creep strains measured during the 7 year loading period are reported. Deflection and strain recoveries due to removal of the loads and for 64 days after load removal as well as the final failure loads for the beams are reported.