Freezing and Thawing Tests of Lightweight Aggregate Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Freezing and Thawing Tests of Lightweight Aggregate Concrete

Author(s): Paul Klieger and J. A. Hanson

Publication: Journal Proceedings

Volume: 57

Issue: 1

Appears on pages(s): 779-796

Keywords: none

DOI: 10.14359/8046

Date: 1/1/1961

Abstract:
Nine lightweight aggregates and one natural sand and gravel aggregate were used in concretes subjected to laboratory freezing and thawing tests and in some cases, to tests for resistance to deicer scaling. Concretes were prepared at two levels of compressivs strength: 3000 psi and 4500 psi at 28 days. Both non-air-entrained and air-entrained concretes were prepared, using the aggregates in on air-dried condition and in a 24-hr saturated condi-tion. The results of these tests indicate the necessity for providing intentionally entrained air to attain a high level of durability, the importance of moisture content of aggregate and then influence of strength level, water-cement ratio, on the durability. The results point to the desirability of evaluating a lightweight aggregate by means of laboratory freezing and thawing tests of air-entrained concrete made with the aggregate, as is gen-erally done for normal weight aggregate.