Reconsolidation Improves Grouted Masonry Wall Panels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reconsolidation Improves Grouted Masonry Wall Panels

Author(s): Manley W. Sahlberg

Publication: Journal Proceedings

Volume: 57

Issue: 12

Appears on pages(s): 689-696

Keywords: none

DOI: 10.14359/8041

Date: 12/1/1960

Abstract:
The type of wall described is actually a reinforced concrete wall cast between bricks or masonry units which act as absorptive forms. It satisfies architects who like brick facings and it also use these walls to resist quakes. satisfies engineers who want to lateral forces induced by earth-The test described was started to demonstrate the practicability of high lift grouting of cavity masonry walls. Some panels were made without vibration, some used vibration or tamping, and others utilized vibration and revi bration.