High-Strength Deformed Steel Bars for Concrete Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High-Strength Deformed Steel Bars for Concrete Reinforcement

Author(s): Sidney A. Guralnick

Publication: Journal Proceedings

Volume: 57

Issue: 9

Appears on pages(s): 241-282

Keywords: none

DOI: 10.14359/8020

Date: 9/1/1960

Abstract:
Results obtained from the testing to destruction of 42 T-beams reinforced with metallurgically-produced high-strength steel deformed bars are presented. Both flexural and shearing failures occurred and the results are compared with the ultimate strength design procedure given in the appendix of the 1956 ACI Building Code and certain other design procedures. Deflections of test beams are compared with values obtained by use of existing methods for computing deflections. Crack data is also reported and evaluated.