Abstract:
The use of adhesives and binders containing epoxy resins by California Division of Highways in repairing concrete is described. Illustrations of their use in repair work are given . The discussion includes possible variations in formulation to secure wanted properties for specific uses, methods of application that are necessary to obtain strong and durable repairs, and a typical formulation for general use.