Title: Tie Requirements for Reinforced Concrete Columns

Author(s): B. Bresler and P. H. Gilbert

Publication: Journal Proceedings

Volume: 58

Issue: 11

Appears on pages(s): 555-570

Keywords: none

DOI: 10.14359/7997

Date: 11/1/1961

Abstract:
Mechanism of failure of reinforced concrete columns with lateral ties is described. Rational criteria for spacing and size of lateral ties are derived, and pilot tests verifying some of these criteria are described.