Title: Strength of Concrete Under Combined Stress

Author(s): C. J. Bellamy

Publication: Journal Proceedings

Volume: 58

Issue: 10

Appears on pages(s): 367-382

Keywords: none

DOI: 10.14359/7989

Date: 10/1/1961

Abstract:
The effect of the intermediate principal stress on the strength of mortar was established for the particular case where the smallest principal stress was zero, by testing hollow cylinders to failure under axial load and confining pressure. The results are compared with some existrng failure criteria, and the graphical system of presentation of the criteria examined critically.