Ultimate Strength Design of Sectionse Controlled by Tension

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ultimate Strength Design of Sectionse Controlled by Tension

Author(s): f. p. Wiesinger and W. T. Marshall

Publication: Journal Proceedings

Volume: 59

Issue: 4

Appears on pages(s): 551-562

Keywords: none

DOI: 10.14359/7928

Date: 4/1/1962

Abstract:
Presents a simplified method of ultimate strength design of rectangular or T-sections controlled by tension. Method applies to sections with or without compressive reinforcement for conditions of bending only or bending with axial load. Equations are presented which express first principles and a universal design chart is given. The method conforms to the requirements of ACI 318-56 and incorporates all the limitations prescribed therein.