Modulus of Elasticity iof Concrete Affected by Elastic Moduli of Cement Paste Matrix and Aggregate

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modulus of Elasticity iof Concrete Affected by Elastic Moduli of Cement Paste Matrix and Aggregate

Author(s): Teddy J. Hirsch

Publication: Journal Proceedings

Volume: 59

Issue: 3

Appears on pages(s): 427-452

Keywords: none

DOI: 10.14359/7924

Date: 3/1/1962

Abstract:
A general equation is derived which expresses the modulus of elasticity of concrete or mortar in terms of an empirical constant the elastic moduli of the cement matrix and aggregate constituents, and the mix proportions. Labo-ratory tests showed the equation to produce good results over a wide range of variables. The average deviation was found to be written lO percent, and the maximum deviation was within 35 percent. The variety of aggregate materials used included steel punchings, crushed glass, lead drops, Ottawa sand, crushed limestone and a calcareous-siliceous river gravel.