Preliminary Study of the Effects of Water-Reducing Retarders on the Strength, Air Void Characteristics, and Durability of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Preliminary Study of the Effects of Water-Reducing Retarders on the Strength, Air Void Characteristics, and Durability of Concrete

Author(s): Thomas D. Larson, John L. Mangusi an dRaymond R. Radomski

Publication: Journal Proceedings

Volume: 60

Issue: 12

Appears on pages(s): 1739-1754

Keywords:

DOI: 10.14359/7912

Date: 12/1/1963

Abstract:
Concretes made with water-reducing retarders showed improved freeze-thaw durability, primarily as a result of increased strength. Specimens made from constant slump, constant cement factor mixtures containing several agents at various dosage levels had higher flexural and comressive strengths than control speciments strengths at 7 and Q8 days correlated significantly with durability factor. Microscopic studies indicated that there were minor differences between the air void systems of control and test concretes. In particular, spacing factors increased with retardation. This appeared to result from. ajr.entrainment by the water-reducing retarders and from bubble dissolution.




  